Technical Specifications
Physical & Mechanical Properties |
Test Method |
Typical Values |
|
1 |
Specific Gravity |
ASTM D2395 |
1.07 - 1.10 |
2 |
Abrasion Resistance |
ASTM D2394 |
0.01"/1000 rev |
3 |
Compression 1 (Parallel) |
ASTM D198 |
2,635 psi |
4 |
Compression 2 (Perpendicular) |
ASTM D198 |
3,864 psi |
5 |
Tensile Strength (Parallel) |
ASTM D198 |
1,189 psi |
6 |
Shear Strength (Longitudinal) |
ASTM D143 |
1,010 psi |
7 |
Modulus of Rupture |
ASTM D4761 |
2,547 psi |
8 |
Modulus of Elasticity |
ASTM D4761 |
361,999 psi |
9 |
Hardness |
ASTM D143 |
1,200 lbs |
10 |
Nail Withdrawal 3 |
ASTM D1761 |
145 lbs/in. |
11 |
Screw Withdrawal 4 |
ASTM D1761 |
435 lbs/in. |
12 |
Water Absorption (Sanded) |
ASTM D1037 |
1.60% |
13 |
Water Absorption (Unsanded) |
ASTM D1037 |
1.05% |
14 |
Coefficient of Friction - Wet |
ASTM D2047 |
0.96 |
15 |
Coefficient of Friction - Dry |
ASTM D2047 |
0.88 |
|
|||
|
DURABILITY |
|
|
16 |
Fungal Resistance - White Rot |
ASTM D1413 |
No Decay |
17 |
Fungal Resistance - Brown Rot |
ASTM D1413 |
No Decay |
18 |
Termite Resistance |
ASTM D3345 |
Rating = 9.6/10 |
|
|||
|
THERMAL |
|
|
19 |
Thermal Expansion |
ASTM E228 |
20.7 x 10^-6 (in/in/°F) |
|
|||
|
FIRE |
|
|
20 |
Self Ignition Temperature |
ASTM D1929 |
874°F |
21 |
Flash Ignition Temperature |
ASTM D1929 |
834°F |
22 |
Flame Spread |
ASTM E84 |
126.32 |
Note: 1. Compression values are obtained from compressive strength parallel and perpendicular to length. 2. Nails must have a diameter less than or equal to that of a 16d common nail. 3. Galvanized No.10 deck screw 2½ inches long. 4. Follow EverGrain installation instructions. Values shown are for reference only and are not meant for design analysis. Typical values obtained under ambient temperature conditions (70°F).